NUKLEONIKA 2004, 49(Supplement 3):s7-s11
Aneta Hanc, Janusz E. Fr¹ckowiak
Institute of Materials Science, University of Silesia, 12 Bankowa Str., 40-007 Katowice, Poland
 
In the present work, the Fe-Al-X (X = Cu; Ni; Cr) metallic powders produced by the self-decomposition 
method of the Fe-Al doped alloys were examined by Mössbauer spectroscopy. The concentration of the Fe 
vacancies and the Fe atoms substituting Al (Fe-AS) was determined from the intensities of the 
sub-spectra in the Mössbauer analysis connected with distinct Fe environments. The results have shown
 that nickel and copper cause an increase of vacancy concentrations in comparison with the values
 found for Fe-Al metallic powders, whereas chromium decreases vacancy concentrations causing 
a significant increase of anti-site atoms Fe-AS concentration.